Study on the Reoxidation Characteristics of Soaked and Air-Dried CoalSource: Journal of Energy Resources Technology:;2019:;volume( 141 ):;issue: 002::page 22203DOI: 10.1115/1.4041407Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: After coal seam mining, the residual coal is soaked with the accumulated water in goaf, and its spontaneous combustion characteristics were changed after air-dried. To study the reoxidation characteristics of soaked and air-dried coal, temperature-programmed experiments were carried out, and the cross point temperatures and index gases were investigated. Results showed that the cross point temperature of raw coal (146.3 °C) was reduced to 137.1 °C after it was pre-oxidized at 90 °C. The cross point temperature of water-soaked, and air-dried coal (96 h) was 122.5 °C, while the cross point temperature of water-soaked, air-dried (96 h) and pre-oxidized (90 °C) coal was 111.5 °C. Although CO was produced in the initial slow oxidation phase, it was found that C2H4 and C3H8 were not generated. In the rapid oxidation stage, different pretreatments affected the gas generation and the overall oxidative degree was consistent with the cross point temperature. The generation temperature and the concentration of C2H4 and C3H8 were decreased after the coal was water-soaked, air-dried, and pre-oxidized. Furthermore, the high-energy chemicals and functional groups were studied, which could be used to explain the physical experiment oxidation characteristics of different coals.
|
Collections
Show full item record
contributor author | Sun, Lulu | |
contributor author | Zhang, Yanbo | |
contributor author | Wang, Yue | |
contributor author | Liu, Qiqi | |
date accessioned | 2019-03-17T10:00:23Z | |
date available | 2019-03-17T10:00:23Z | |
date copyright | 9/26/2018 12:00:00 AM | |
date issued | 2019 | |
identifier issn | 0195-0738 | |
identifier other | jert_141_02_022203.pdf | |
identifier uri | http://yetl.yabesh.ir/yetl1/handle/yetl/4255853 | |
description abstract | After coal seam mining, the residual coal is soaked with the accumulated water in goaf, and its spontaneous combustion characteristics were changed after air-dried. To study the reoxidation characteristics of soaked and air-dried coal, temperature-programmed experiments were carried out, and the cross point temperatures and index gases were investigated. Results showed that the cross point temperature of raw coal (146.3 °C) was reduced to 137.1 °C after it was pre-oxidized at 90 °C. The cross point temperature of water-soaked, and air-dried coal (96 h) was 122.5 °C, while the cross point temperature of water-soaked, air-dried (96 h) and pre-oxidized (90 °C) coal was 111.5 °C. Although CO was produced in the initial slow oxidation phase, it was found that C2H4 and C3H8 were not generated. In the rapid oxidation stage, different pretreatments affected the gas generation and the overall oxidative degree was consistent with the cross point temperature. The generation temperature and the concentration of C2H4 and C3H8 were decreased after the coal was water-soaked, air-dried, and pre-oxidized. Furthermore, the high-energy chemicals and functional groups were studied, which could be used to explain the physical experiment oxidation characteristics of different coals. | |
publisher | The American Society of Mechanical Engineers (ASME) | |
title | Study on the Reoxidation Characteristics of Soaked and Air-Dried Coal | |
type | Journal Paper | |
journal volume | 141 | |
journal issue | 2 | |
journal title | Journal of Energy Resources Technology | |
identifier doi | 10.1115/1.4041407 | |
journal fristpage | 22203 | |
journal lastpage | 022203-6 | |
tree | Journal of Energy Resources Technology:;2019:;volume( 141 ):;issue: 002 | |
contenttype | Fulltext |