YaBeSH Engineering and Technology Library

    • Journals
    • PaperQuest
    • YSE Standards
    • YaBeSH
    • Login
    View Item 
    •   YE&T Library
    • ASME
    • Journal of Applied Mechanics
    • View Item
    •   YE&T Library
    • ASME
    • Journal of Applied Mechanics
    • View Item
    • All Fields
    • Source Title
    • Year
    • Publisher
    • Title
    • Subject
    • Author
    • DOI
    • ISBN
    Advanced Search
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Archive

    Interface Fracture: Failure Criteria

    Source: Journal of Applied Mechanics:;2020:;volume( 087 ):;issue: 005
    Author:
    Banks-Sills, Leslie
    DOI: 10.1115/1.4046198
    Publisher: The American Society of Mechanical Engineers (ASME)
    Abstract: Failure criteria for a crack between two dissimilar materials are presented. Test data from three different material pairs are considered. The first two consist of an interface crack between glass and epoxy and two dissimilar ceramic clays. For the third material pair, there is a delamination between two unidirectional carbon fiber polymer-reinforced plies with fibers in the 0 deg and 90 deg directions. Failure criteria for these materials have been presented previously. In this study, invariant parameters are used in the failure criteria. It is seen that the invariant length parameter has values which are unrealistically large and small. The preferred criterion is based on first principles.
    • Download: (625Kb)
    • Show Full MetaData Hide Full MetaData
    • Get RIS
    • Item Order
    • Go To Publisher
    • Statistics

      Interface Fracture: Failure Criteria

    URI
    https://yetl.yabesh.ir/yetl1/handle/yetl/4274388
    Collections
    • Journal of Applied Mechanics

    Show full item record

    contributor authorBanks-Sills, Leslie
    date accessioned2022-02-04T14:47:48Z
    date available2022-02-04T14:47:48Z
    date copyright2020/02/14/
    date issued2020
    identifier issn0021-8936
    identifier otherjam_87_5_051007.pdf
    identifier urihttp://yetl.yabesh.ir/yetl1/handle/yetl/4274388
    description abstractFailure criteria for a crack between two dissimilar materials are presented. Test data from three different material pairs are considered. The first two consist of an interface crack between glass and epoxy and two dissimilar ceramic clays. For the third material pair, there is a delamination between two unidirectional carbon fiber polymer-reinforced plies with fibers in the 0 deg and 90 deg directions. Failure criteria for these materials have been presented previously. In this study, invariant parameters are used in the failure criteria. It is seen that the invariant length parameter has values which are unrealistically large and small. The preferred criterion is based on first principles.
    publisherThe American Society of Mechanical Engineers (ASME)
    titleInterface Fracture: Failure Criteria
    typeJournal Paper
    journal volume87
    journal issue5
    journal titleJournal of Applied Mechanics
    identifier doi10.1115/1.4046198
    page51007
    treeJournal of Applied Mechanics:;2020:;volume( 087 ):;issue: 005
    contenttypeFulltext
    DSpace software copyright © 2002-2015  DuraSpace
    نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
    yabeshDSpacePersian
     
    DSpace software copyright © 2002-2015  DuraSpace
    نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
    yabeshDSpacePersian