description abstractFailure criteria for a crack between two dissimilar materials are presented. Test data from three different material pairs are considered. The first two consist of an interface crack between glass and epoxy and two dissimilar ceramic clays. For the third material pair, there is a delamination between two unidirectional carbon fiber polymer-reinforced plies with fibers in the 0 deg and 90 deg directions. Failure criteria for these materials have been presented previously. In this study, invariant parameters are used in the failure criteria. It is seen that the invariant length parameter has values which are unrealistically large and small. The preferred criterion is based on first principles.
publisherThe American Society of Mechanical Engineers (ASME)
titleInterface Fracture: Failure Criteria
typeJournal Paper
journal volume87
journal issue5
journal titleJournal of Applied Mechanics
identifier doi10.1115/1.4046198
page51007
treeJournal of Applied Mechanics:;2020:;volume( 087 ):;issue: 005
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record