Show simple item record

dc.contributor.authorPhuc Nguyen-Duy
dc.contributor.authorSerge Bayard
dc.date.accessioned2017-05-08T23:11:17Z
dc.date.available2017-05-08T23:11:17Z
dc.date.copyrightJanuary, 1981
dc.date.issued1981
dc.identifier.issn0094-4289
dc.identifier.otherJEMTA8-26880#55_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/94650
dc.description.abstractThe fracture-energy criterion JIc was determined by the single specimen method on quenched and tempered 4130 steel used for tower anchor bars of high voltage transmission lines. A thermodynamic approach was used to rationalize JIc as a stable crack initiation criterion. Slow-bend testing was performed on three-point bend specimens of different dimensions. The effect of microstructure (martensite and bainite + ferrite) on the value of JIc is not significant. Specimen dimensions (1.5 × 3 × 15 cm; 2 × 4 × 20 cm) seem not to affect JIc values. Critical stretch zone width, WSZc , was evaluated on broken specimen halves using scanning electron microscopy. With some assumptions, relationships between WSZc , CTOD and JIc were established. Values of JIc calculated via WSZc compare favorably with JIc determined from a single specimen.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFracture Toughness of 4130 Quenched and Tempered Steel
dc.typeJournal Paper
dc.journal.volume103
dc.journal.issue1
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3224972
dc.journal.fristpage55
dc.journal.lastpage61
dc.identifier.eissn1528-8889
dc.keywordsSteel
dc.keywordsFracture toughness
dc.keywordsDimensions
dc.keywordsFerrites (Magnetic materials)
dc.keywordsFracture (Process)
dc.keywordsScanning electron microscopy
dc.keywordsTesting
dc.keywordsTransmission lines AND Electric potential
dc.treeJournal of Engineering Materials and Technology:;1981:;volume( 103 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record