Show simple item record

dc.contributor.authorLam, Poh
dc.contributor.authorSindelar, Robert L.
dc.date.accessioned2017-05-09T01:32:47Z
dc.date.available2017-05-09T01:32:47Z
dc.date.issued2016
dc.identifier.issn0094-9930
dc.identifier.otherpvt_138_04_041406.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/162368
dc.description.abstractA typical multipurpose canister (MPC) is made of austenitic stainless steel and is loaded with spent nuclear fuel (SNF) assemblies. Because heat treatment for stress relief is not required for the construction of the MPC, the canister is susceptible to stress corrosion cracking in the weld or heat affected zone (HAZ) regions under longterm storage conditions. Logic for flaw acceptance is developed should cracklike flaws be detected by Inservice Inspection. The procedure recommended by API 5791/ASME FFS1, FitnessforService, is used to calculate the instability crack length or depth by failure assessment diagram (FAD). It is demonstrated that the welding residual stress (RS) has a strong influence on the results.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFlaw Stability Considering Residual Stress for Aging Management of Spent Nuclear Fuel Multiple Purpose Canisters
dc.typeJournal Paper
dc.journal.volume138
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4032279
dc.journal.fristpage41406
dc.journal.lastpage41406
dc.identifier.eissn1528-8978
dc.treeJournal of Pressure Vessel Technology:;2016:;volume( 138 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record