dc.description.abstractThis paper describes a sequence of residual stress measurements made to determine a twodimensional map of biaxial residual stress in a nozzle mockup having two welds, one a dissimilar metal (DM) weld and the other a stainless steel (SS) weld. The mockup is cylindrical, designed to represent a pressurizer surge nozzle of a nuclear pressurized water reactor (PWR), and was fabricated as part of a weld residual stress measurement and finiteelement (FE) modeling roundrobin exercise. The mockup has a nickel alloy DM weld joining an SS safe end to a lowalloy steel cylinder and stiffening ring, as well as an SS weld joining the safe end to a section of SS pipe. The biaxial mapping experiments follow an approach described earlier, in PVP201278885 and PVP201397246, and comprise a series of experimental steps and a computation to determine a twoآ dimensional map of biaxial (axial and hoop) residual stress near the SS and DM welds. Specifically, the biaxial stresses are a combination of a contour measurement of hoop stress in the cylinder, slitting measurements of axial stress in thin slices removed from the cylinder wall, and a computation that determines the axial stress induced by measured hoop stress. At the DM weld, hoop stress is tensile near the OD (240 MPa) and compressive at the ID (−320 MPa), and axial stress is tensile near the OD (370 MPa) and compressive near the midthickness (−230 MPa) and ID (−250 MPa). At the SS weld, hoop stress is tensile near the OD (330 MPa) and compressive near the ID (−210 MPa), and axial stress is tensile at the OD (220 MPa) and compressive near midthickness (−225 MPa) and ID (−30 MPa). The measured stresses are found to be consistent with earlier work in similar configurations.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleBiaxial Residual Stress Mapping for a Dissimilar Metal Welded Nozzle
dc.typeJournal Paper
dc.journal.volume138
dc.journal.issue1
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4031504
dc.journal.fristpage11404
dc.journal.lastpage11404
dc.identifier.eissn1528-8978
dc.treeJournal of Pressure Vessel Technology:;2016:;volume( 138 ):;issue: 001