    Effect of Weld Residual Stress Fitting on Stress Intensity Factor for Circumferential Surface Cracks in Pipe

    Thumbnail
    View/Open
    pvt_137_01_011403.pdf (2.639Mb)
    Date
    2015
    Author
    Shim, Do
    Xu, Steven
    Kerr, Matthew
    Metadata
    Show full item record
    Abstract
    Recent studies have shown that the crack growth of primary water stress corrosion cracking (PWSCC) is mainly driven by the weld residual stress (WRS) within the dissimilar metal weld. The existing stress intensity factor (K) solutions for surface cracks in pipe typically require a fourth order polynomial stress distribution through the pipe wall thickness. However, it is not always possible to accurately represent the through thickness WRS with a fourth order polynomial fit and it is necessary to investigate the effect of the WRS fitting on the calculated Ks. In this paper, two different methods were used to calculate the K for a semielliptical circumferential surface crack in a pipe under a given set of simulated WRS. The first method is the universal weight function method (UWFM) where the through thickness WRS distribution is represented as a piecewise monotonic cubic fit. In the second method, the through thickness WRS profiles are represented as a fourth order polynomial curve fit (both using the entire wall thickness data and only using data up to the cracktip). In addition, threedimensional finite element (FE) analyses (using the simulated weld residual stress) were conducted to provide a reference solution. The results of this study demonstrate the potential sensitivity of Ks to fourth order polynomial fitting artifacts. The piecewise WRS representations used in the UWFM were not sensitive to these fitting artifacts and the UWFM solutions were in good agreement with the FE results. In addition, in certain cases, it was demonstrated that more accurate crack growth calculations of PWSCC are made when the UWFM is used.
    URI
    http://yetl.yabesh.ir/yetl/handle/yetl/159430
    Collections
    • Journal of Pressure Vessel Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV