dc.contributor.authorE. Citirik
dc.date.accessioned2017-05-09T00:54:02Z
dc.date.available2017-05-09T00:54:02Z
dc.date.copyrightJune, 2012
dc.date.issued2012
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28567#031202_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/150112
dc.description.abstractA comprehensive methodology is developed to understand and characterize the fracture behavior of circumferentially cracked boiler tubes in this study. Weld overlay is applied on the coal-fired boiler tubes in order to prevent the degradation of corrosive and erosive environment that the boiler tubes are exposed to in the power plants. Finite element modeling and analysis are employed for all of the computations including steady-state and transient stress intensity factor (SIF) calculations in this study. Circumferential cracking has been one of the failure modes in waterwall boiler tubes, which results in high maintenance and replacement costs. Thermomechanical stresses and corrosive environment are basically the two remarkable contributors that bring about this failure mode. The former one is investigated and quantified in this study in order to explain the fracture behavior of weld overlay coatings during the power plant operation. Periodic soot blowing operations cause cyclic transient thermomechanical stresses on the weld overlay coating that results in crack propagation and fatigue failure. Three-dimensional fracture analysis of circumferentially cracked boiler tubes is examined using enriched finite element method in this study. Transient temperatures and thermomechanical stresses are computed using ANSYS for five different periodic crack spacing values (h), which are 2, 4, 6, 10, and 20 mm in the axial direction. 3D fracture analysis was performed, and stress intensity factors were computed using FRAC3D , which is Finite Element Analysis (FEA) software developed at Lehigh University. The maximum stress intensity factor is obtained at the deepest penetration of the crack in the model which has the largest periodic axial crack spacing, h = 20 mm. The stress intensity factors due to welding residuals decrease as the axial crack spacing, h, decreases. The FEA methodology developed in this research would provide the engineers with the ability to understand the fracture problem and predict component life and improve the reliability of the weld overlay coated boiler tubes utilized in the power plants.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleThree-Dimensional Fracture Analysis of Circumferentially Cracked Boiler Tubes
dc.typeJournal Paper
dc.journal.volume134
dc.journal.issue3
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4005857
dc.journal.fristpage31202
dc.identifier.eissn1528-8978
dc.keywordsTemperature
dc.keywordsStress
dc.keywordsFracture (Process)
dc.keywordsSteady state
dc.keywordsBoiler tubes
dc.keywordsOverlays (Materials engineering)
dc.keywordsThermal stresses
dc.keywordsFinite element analysis
dc.keywordsWelding
dc.keywordsSoot AND Computation
dc.treeJournal of Pressure Vessel Technology:;2012:;volume( 134 ):;issue: 003