dc.description.abstractBlunt notch fatigue crack initiation tests for Type A387 2.25 Cr-1 Mo steel and 316L stainless steel were performed in air at room temperature, in silicone oil at room temperature, in V-131B coal process solvent at 100°C, and in chlorine-modified V-131B coal process solvent at 100°C. For both steels the most damaging environment was room temperature air. The number of cycles to initiate a crack were almost identical in the coal process solvent and the silicone oil for the Type A-387 steel. These two environments resulted in the longest crack initiation lifetime for the Type A-387 steel. The crack initiation lifetime for the Type A-387 steel in the chlorine modified V-131 B coal process solvent was roughly a factor of five less than the lifetime in the silicone oil and the unmodified coal process solvent. The crack initiation lifetime for the Type A-387 steel in room temperature air was a factor of 30 less than the lifetime in the silicone oil or the unmodified coal process solvent. The improvement of the crack initiation lifetime for the Type A-387 steel in the unmodified coal process solvent and the silicone oil is attributed to protection of the material from embrittlement from room temperature air. The decrease in crack initiation lifetime in the chlorine modified coal process solvent indicates that chlorine can be an active embrittling agent in the coal process solvent. The crack initiation lifetime for 316L stainless steel was longest in the silicone oil. The lifetime decreased somewhat in the unmodified coal process solvent with a further decrease for the chlorine modified coal solvent. The crack initiation lifetime in air was an order of magnitude lower than the lifetime in the silicone oil. The silicone oil and the coal process solvent apparently protected the 316L stainless from the embrittlement in air. However, the coal process solvent is not entirely inert as in the case of Type A-387 steel. The chlorine is an active embrittling agent for the 316L stainless steel in the coal process solvent.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleEnvironmental Effects on Fatigue Crack Initiation in 2.25 Cr-1 Mo Steel and 316L Stainless Steel
dc.typeJournal Paper
dc.journal.volume110
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3226043
dc.journal.fristpage240
dc.journal.lastpage246
dc.identifier.eissn1528-8889
dc.keywordsSteel
dc.keywordsFatigue cracks
dc.keywordsStainless steel
dc.keywordsCoal
dc.keywordsFracture (Materials)
dc.keywordsSilicones
dc.keywordsTemperature
dc.keywordsEmbrittlement AND Cycles
dc.treeJournal of Engineering Materials and Technology:;1988:;volume( 110 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record