    Environmental Effects on Fatigue Crack Initiation in 2.25 Cr-1 Mo Steel and 316L Stainless Steel

    Thumbnail
    View/Open
    JEMTA8-26922#240_1.pdf (2.575Mb)
    Date
    1988
    Author
    V. K. Mathews
    T. S. Gross
    Metadata
    Show full item record
    Abstract
    Blunt notch fatigue crack initiation tests for Type A387 2.25 Cr-1 Mo steel and 316L stainless steel were performed in air at room temperature, in silicone oil at room temperature, in V-131B coal process solvent at 100°C, and in chlorine-modified V-131B coal process solvent at 100°C. For both steels the most damaging environment was room temperature air. The number of cycles to initiate a crack were almost identical in the coal process solvent and the silicone oil for the Type A-387 steel. These two environments resulted in the longest crack initiation lifetime for the Type A-387 steel. The crack initiation lifetime for the Type A-387 steel in the chlorine modified V-131 B coal process solvent was roughly a factor of five less than the lifetime in the silicone oil and the unmodified coal process solvent. The crack initiation lifetime for the Type A-387 steel in room temperature air was a factor of 30 less than the lifetime in the silicone oil or the unmodified coal process solvent. The improvement of the crack initiation lifetime for the Type A-387 steel in the unmodified coal process solvent and the silicone oil is attributed to protection of the material from embrittlement from room temperature air. The decrease in crack initiation lifetime in the chlorine modified coal process solvent indicates that chlorine can be an active embrittling agent in the coal process solvent. The crack initiation lifetime for 316L stainless steel was longest in the silicone oil. The lifetime decreased somewhat in the unmodified coal process solvent with a further decrease for the chlorine modified coal solvent. The crack initiation lifetime in air was an order of magnitude lower than the lifetime in the silicone oil. The silicone oil and the coal process solvent apparently protected the 316L stainless from the embrittlement in air. However, the coal process solvent is not entirely inert as in the case of Type A-387 steel. The chlorine is an active embrittling agent for the 316L stainless steel in the coal process solvent.
    URI
    http://yetl.yabesh.ir/yetl/handle/yetl/103963
    Collections
    • Journal of Engineering Materials and Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV