description abstractThe effect of a girth-weld-induced residual stress field on the linear elastic fracture mechanics of a thin-walled pipe is examined. The procedure for using the residual stress distribution to compute KI and KII for a circumferential crack which is growing radially is described. In addition to the two-pass girth weld, stress intensity factors are computed for a residual stress distribution in a flat plate and for a hypothetical residual stress state in a second thin-walled pipe. The computed stress intensity factor for the flat plate geometry and its residual stress distribution are compared with a solution from the literature as a check on the computational procedure. The through-the-thickness residual stress distribution due to the two-pass girth weld is similar to a half-cosine wave. For purposes of comparison, the hypothetical through-the-thickness distribution selected for the second pipe is similar to a full cosine wave. The stress intensity factor is presented as a function of crack depth for a crack initiating on the inner surface of the pipe. The redistribution of residual stresses due to crack growth is also shown for selected crack lengths. The study shows that residual stress-induced crack growth in pipes can be significantly different from that in flat plates due to the possibility of locked-in residual bending moments in the pipe. These locked-in moments can have effects similar to externally applied loads and can either promote or restrain crack growth. A residual stress distribution is illustrated in which crack growth, if initiated, would continue through the entire wall. Also, a residual stress distribution is illustrated for which the crack could arrest after a certain amount of growth.
publisherThe American Society of Mechanical Engineers (ASME)
titleStress Intensity Factors due to Residual Stresses in Thin-Walled Girth-Welded Pipes
typeJournal Paper
journal volume103
journal issue1
journal titleJournal of Pressure Vessel Technology
identifier doi10.1115/1.3263372
journal fristpage66
journal lastpage75
identifier eissn1528-8978
keywordsResidual stresses
keywordsStress
keywordsPipes
keywordsFracture (Materials)
keywordsStress concentration
keywordsFlat plates
keywordsThickness
keywordsWaves
keywordsFracture mechanics AND Geometry
treeJournal of Pressure Vessel Technology:;1981:;volume( 103 ):;issue: 001
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record