Response of Beam-To-Column Web Cleated Joints For FRP Pultruded MembersSource: Journal of Composites for Construction:;2014:;Volume ( 018 ):;issue: 002DOI: 10.1061/(ASCE)CC.1943-5614.0000392Publisher: American Society of Civil Engineers
Abstract: Physical testing is used to characterize the structural properties of beam-to-column joints, comprising pultruded fiber-reinforced polymer (FRP) H-shapes of depth 203 mm, connected by 128 mm-long web cleats and two M16 bolts per leg. Testing is performed on two batches of nominally identical specimens. One batch had web cleats of pultruded FRP and the other had structural steel. The structural behavior of the joints is based on their moment-rotation responses, failure modes, and serviceability vertical deflection limits. Joints with FRP cleats failed by delamination cracking at the top of the cleats, and when the cleats were of steel, the FRP failure occurred inside the column members. Neither failure mode is reported in the design manuals from pultruders. At the onset of the FRP damage, it was found that the steel joints were twice as stiff as the FRP joints. On the basis of a characteristic (damage) rotation, calculated in accordance with Eurocode 0, the serviceability deflection limits are established to be span/300 and span/650 for the joints with FRP and steel cleats, respectively. This finding suggests that appropriate deflection limits, in relation to cleated connections, should be proposed in manufactures’ design manuals and relative design standards and design codes. Failure to address the serviceability, by the engineer of record, could lead to unreliable designs.
|
Collections
Show full item record
contributor author | Jawed Qureshi | |
contributor author | J. Toby Mottram | |
date accessioned | 2017-05-08T21:36:51Z | |
date available | 2017-05-08T21:36:51Z | |
date copyright | April 2014 | |
date issued | 2014 | |
identifier other | %28asce%29cc%2E1943-5614%2E0000395.pdf | |
identifier uri | http://yetl.yabesh.ir/yetl/handle/yetl/57536 | |
description abstract | Physical testing is used to characterize the structural properties of beam-to-column joints, comprising pultruded fiber-reinforced polymer (FRP) H-shapes of depth 203 mm, connected by 128 mm-long web cleats and two M16 bolts per leg. Testing is performed on two batches of nominally identical specimens. One batch had web cleats of pultruded FRP and the other had structural steel. The structural behavior of the joints is based on their moment-rotation responses, failure modes, and serviceability vertical deflection limits. Joints with FRP cleats failed by delamination cracking at the top of the cleats, and when the cleats were of steel, the FRP failure occurred inside the column members. Neither failure mode is reported in the design manuals from pultruders. At the onset of the FRP damage, it was found that the steel joints were twice as stiff as the FRP joints. On the basis of a characteristic (damage) rotation, calculated in accordance with Eurocode 0, the serviceability deflection limits are established to be span/300 and span/650 for the joints with FRP and steel cleats, respectively. This finding suggests that appropriate deflection limits, in relation to cleated connections, should be proposed in manufactures’ design manuals and relative design standards and design codes. Failure to address the serviceability, by the engineer of record, could lead to unreliable designs. | |
publisher | American Society of Civil Engineers | |
title | Response of Beam-To-Column Web Cleated Joints For FRP Pultruded Members | |
type | Journal Paper | |
journal volume | 18 | |
journal issue | 2 | |
journal title | Journal of Composites for Construction | |
identifier doi | 10.1061/(ASCE)CC.1943-5614.0000392 | |
tree | Journal of Composites for Construction:;2014:;Volume ( 018 ):;issue: 002 | |
contenttype | Fulltext |