Show simple item record

contributor authorTao Zhang
contributor authorJinsuo Nie
contributor authorSyed A. Ali
contributor authorCharles H. Hofmayer
contributor authorFrederick W. Brust
contributor authorGery Wilkowski
contributor authorDo-Jun Shim
date accessioned2017-05-09T00:54:15Z
date available2017-05-09T00:54:15Z
date copyrightFebruary, 2012
date issued2012
identifier issn0094-9930
identifier otherJPVTAS-28556#011801_1.pdf
identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/150183
description abstractNuclear power plant safety under seismic conditions is an important consideration. The piping systems may have some defects caused by fatigue, stress corrosion cracking, etc., in aged plants. These cracks may not only affect the seismic response but also grow and break through causing loss of coolant. Therefore, an evaluation method needs to be developed to predict crack growth behavior under seismic excitation. This paper describes efforts conducted to analyze and better understand a series of degraded pipe tests under seismic loading that was conducted by Japan Nuclear Energy Safety Organization (JNES). A special “cracked-pipe element” (CPE) concept, where the element represented the global moment-rotation response due to the crack, was developed. This approach was developed to significantly simplify the dynamic finite element analysis in fracture mechanics fields. In this paper, model validation was conducted by comparisons with a series of pipe tests with circumferential through-wall and surface cracks under different excitation conditions. These analyses showed that reasonably accurate predictions could be made using the abaqus connector element to model the complete transition of a circumferential surface crack to a through-wall crack under cyclic dynamic loading. The JNES primary loop recirculation piping test was analyzed in detail. This combined-component test had three crack locations and multiple applied simulated seismic block loadings. Comparisons were also made between the ABAQUS finite element (FE) analyses results to the measured displacements in the experiment. Good agreement was obtained, and it was confirmed that the simplified modeling is applicable to a seismic analysis for a cracked pipe on the basis of fracture mechanics. Pipe system leakage did occur in the JNES tests. The analytical predictions using the CPE approach did not predict leakage, suggesting that cyclic ductile tearing with large-scale plasticity was not the crack growth mode for the acceleration excitations considered here. Hence, the leakage was caused by low-cycle fatigue with small-scale yielding. The procedure used to make predictions of low-cycle fatigue crack growth with small-scale yielding was based on the Dowling ΔJ procedure, which is an extension of linear-elastic fatigue crack growth methodology into the nonlinear plasticity region. The predicted moments from the CPE approach were used using a cycle-by-cycle crack growth procedure. The predictions compare quite well with the experimental measurements.
publisherThe American Society of Mechanical Engineers (ASME)
titleNumerical Analysis of JNES Seismic Tests on Degraded Combined Piping System
typeJournal Paper
journal volume134
journal issue1
journal titleJournal of Pressure Vessel Technology
identifier doi10.1115/1.4005055
journal fristpage11801
identifier eissn1528-8978
keywordsStress
keywordsFracture (Materials)
keywordsPipes
keywordsLow cycle fatigue
keywordsPiping systems
keywordsSurface cracks
keywordsPlasticity
keywordsCycles
keywordsLeakage
keywordsRotation
keywordsNumerical analysis
keywordsFinite element analysis
keywordsFracture mechanics AND Measurement
treeJournal of Pressure Vessel Technology:;2012:;volume( 134 ):;issue: 001
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record