description abstractWith growing understanding of the differences between solid residues from the fluidized bed combustion of petroleum coke and of coal, the significance of fuel-derived and sorbent-derived components of the ash has become clearer. It is well documented that hydration of the ashes is necessary prior to disposal or utilization or as a reactivation method. Initially, hydration of the lime was thought to involve water reacting only with CaO to form Ca(OH)2 but when the free lime content of the ashes is looked at before and after hydration, it is apparent that the process is more complex. Detailed analyses have shown that the free lime can decrease and vary within the same ash in different particle size ranges. The complexity of the reactions is reflected in problems with the assessment of the free lime content of the materials and the effect of hydration on different particle size fractions of the ash. The free lime content of the ash is significantly lower than expected based on the elemental analysis. Bed ash from the circulating fluidized bed combustion boilers owned and operated by the Nelson Industrial Steam Company Ltd. (NISCO) was examined in detail to elucidate the fate of calcium in the ash during hydration, using a range of techniques. The objective of the study is to determine the amount of CaO available for hydration/reactivation and to better understand interactions of Ca and other mineral components of the ash. Analysis results indicate that in NISCO ashes up to about 6% of the analytical CaO may be combined as acid soluble and insoluble OCCs (other calcium compounds). This implies up to about 10% less free lime than would be inferred from standard chemical analyses. About 1% of the missing CaO can be present as acid insoluble Ca and Mg vanadates, with up to 2% bound in soluble OCCs. The remaining 3–4% is still not accounted for. It is clear that even very minor quantities of mineral matter, other than CaO or CaSO4, associated mainly with the coarser size fractions, are important. The amount of bound water in the hydrated ash, other than that combined in portlandite or brucite, can be as large as 3–5%. This cannot be ignored when sample mass change on hydration or heating is used as a measure of the extent of CaO to Ca(OH)2 conversion.
publisherThe American Society of Mechanical Engineers (ASME)
titleUnderstanding the Behavior of Calcium Compounds in Petroleum Coke Fluidized Bed Combustion (FBC) Ash
typeJournal Paper
journal volume128
journal issue4
journal titleJournal of Energy Resources Technology
identifier doi10.1115/1.2358144
journal fristpage290
journal lastpage299
identifier eissn1528-8994
keywordsFuels
keywordsCoke
keywordsFluidized bed combustion
keywordsSorbents
keywordsCoal
keywordsAsh
keywordsParticle size
keywordsPetroleum
keywordsSteam
keywordsWater
keywordsQuartz AND Neutrons
treeJournal of Energy Resources Technology:;2006:;volume( 128 ):;issue: 004
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record