Show simple item record

contributor authorBrunschwiler, Thomas
contributor authorSchlottig, Gerd
contributor authorNi, Songbo
contributor authorLiu, Yu
contributor authorGoicochea, Javier V.
contributor authorZأ¼rcher, Jonas
contributor authorWolf, Heiko
date accessioned2017-05-09T01:06:55Z
date available2017-05-09T01:06:55Z
date issued2014
identifier issn1528-9044
identifier otherep_136_04_041012.pdf
identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/154506
description abstractThis work presents enhanced composite joints that support both electrical and thermal transport in electronic packages. The joints are sequentially formed by applying a nanoparticle suspension, evaporating a solvent, selfassembling of nanoparticles by capillary bridging, and the formation of so called “necksâ€‌ between micrometersized features. This sequence is used to either form low temperature electrical joints under copper pillars or enhanced percolating thermal underfills (ePTU) with areal contacts between filler particles of the composite. The report discusses processing aspects of the capillary bridges evolution and of uniform neck formation, it discusses strategies to achieve mechanically stable necks, and it compares the performance of the achieved joints against stateoftheart solutions. The capillary bridge evolution during liquid evaporation was investigated in copper pillar arrays and random particle beds. The vapor–liquid interface first penetrates locations of low pillar or particle density resulting in a dendritic fluid network. Once the network breaks up, individual necks form. For aqueous nanosuspensions, highly uniform necks with high yield were obtained by evaporation at 60 آ°C. Isothermal conditions were preferred to yield equal neck counts at the cavity's top and bottom surfaces. Mechanically stable silver necks required an annealing at only 150 آ°C, dielectric necks an annealing at 140 آ°C with a bimodal approach. Therein polystyrene (PS) nanoparticles occupy interstitial positions in densly packed alumina necks, then melt and adhere to the alumina. The electrical necks showed a shear strength of 16 MPa, equivalent to silver joints used in power electronic packages. The thermal necks yielded a thermal conductivity of up to 3.8 W/mK, fivefold higher than commercially available capillary thermal underfills.
publisherThe American Society of Mechanical Engineers (ASME)
titleEnhanced Electrical and Thermal Interconnects by the Self Assembly of Nanoparticle Necks Utilizing Capillary Bridging
typeJournal Paper
journal volume136
journal issue4
journal titleJournal of Electronic Packaging
identifier doi10.1115/1.4028332
journal fristpage41012
journal lastpage41012
identifier eissn1043-7398
treeJournal of Electronic Packaging:;2014:;volume( 136 ):;issue: 004