YaBeSH Engineering and Technology Library

    • Journals
    • PaperQuest
    • YSE Standards
    • YaBeSH
    • Login
    View Item 
    •   YE&T Library
    • ASME
    • Journal of Pressure Vessel Technology
    • View Item
    •   YE&T Library
    • ASME
    • Journal of Pressure Vessel Technology
    • View Item
    • All Fields
    • Source Title
    • Year
    • Publisher
    • Title
    • Subject
    • Author
    • DOI
    • ISBN
    Advanced Search
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Archive

    Equivalent CTOD Ratio β for Engineering Assessment of CTOD Correction for Constraint Loss

    Source: Journal of Pressure Vessel Technology:;2012:;volume( 134 ):;issue: 005::page 51403
    Author:
    Mitsuru Ohata
    ,
    Fumiyoshi Minami
    DOI: 10.1115/1.4006346
    Publisher: The American Society of Mechanical Engineers (ASME)
    Abstract: The critical CTOD δWP for structural components associated with plastic constraint loss in case of the brittle fracture over small-scale yielding condition can be corrected from CTOD fracture toughness δ by means of the “equivalent CTOD ratio β” defined as δ/δWP , which is based on the Weibull stress criterion. In this study, taking the case of specific wide plate components subjected to uni-axial tensile load, the effect on β is analyzed taking account of Weibull shape parameter m, loading level, constraint effect that can be influenced by material work-hardening and crack type/size in structural components, etc., and volumetric effect. It is found that the β-value is almost constant beyond the applied CTOD level that is lower than CTOD of small-scale yielding limit (SSY-limit) for 25 mm thick toughness specimen. From an engineering point of view, the β-value at the CTOD level of 0.01 mm is used in the whole loading range beyond SSY-limit CTOD, which provides to some extent conservative measure of fracture toughness of structural components. The defined β is found to decrease with increasing Weibull shape parameter m and yield-to-tensile ratio YR of steel for all type of wide plates concerned. The crack length effect on β is quasi-theoretically formulated, which can convert the β for the wide plate with reference crack size to β for target crack size. These β and quasi-theoretical equations for the correction of crack size effect can be utilized for estimating the CTOD for wide plate in consideration of constraint loss effect without numerical calculation of the Weibull stress.
    keyword(s): Stress , Fracture (Materials) , Fracture toughness , Toughness , Steel AND Shapes ,
    • Download: (1.221Mb)
    • Show Full MetaData Hide Full MetaData
    • Get RIS
    • Item Order
    • Go To Publisher
    • Statistics

      Equivalent CTOD Ratio β for Engineering Assessment of CTOD Correction for Constraint Loss

    URI
    https://yetl.yabesh.ir/yetl1/handle/yetl/150071
    Collections
    • Journal of Pressure Vessel Technology

    Show full item record

    contributor authorMitsuru Ohata
    contributor authorFumiyoshi Minami
    date accessioned2017-05-09T00:53:56Z
    date available2017-05-09T00:53:56Z
    date copyrightOctober, 2012
    date issued2012
    identifier issn0094-9930
    identifier otherJPVTAS-926074#051403_1.pdf
    identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/150071
    description abstractThe critical CTOD δWP for structural components associated with plastic constraint loss in case of the brittle fracture over small-scale yielding condition can be corrected from CTOD fracture toughness δ by means of the “equivalent CTOD ratio β” defined as δ/δWP , which is based on the Weibull stress criterion. In this study, taking the case of specific wide plate components subjected to uni-axial tensile load, the effect on β is analyzed taking account of Weibull shape parameter m, loading level, constraint effect that can be influenced by material work-hardening and crack type/size in structural components, etc., and volumetric effect. It is found that the β-value is almost constant beyond the applied CTOD level that is lower than CTOD of small-scale yielding limit (SSY-limit) for 25 mm thick toughness specimen. From an engineering point of view, the β-value at the CTOD level of 0.01 mm is used in the whole loading range beyond SSY-limit CTOD, which provides to some extent conservative measure of fracture toughness of structural components. The defined β is found to decrease with increasing Weibull shape parameter m and yield-to-tensile ratio YR of steel for all type of wide plates concerned. The crack length effect on β is quasi-theoretically formulated, which can convert the β for the wide plate with reference crack size to β for target crack size. These β and quasi-theoretical equations for the correction of crack size effect can be utilized for estimating the CTOD for wide plate in consideration of constraint loss effect without numerical calculation of the Weibull stress.
    publisherThe American Society of Mechanical Engineers (ASME)
    titleEquivalent CTOD Ratio β for Engineering Assessment of CTOD Correction for Constraint Loss
    typeJournal Paper
    journal volume134
    journal issue5
    journal titleJournal of Pressure Vessel Technology
    identifier doi10.1115/1.4006346
    journal fristpage51403
    identifier eissn1528-8978
    keywordsStress
    keywordsFracture (Materials)
    keywordsFracture toughness
    keywordsToughness
    keywordsSteel AND Shapes
    treeJournal of Pressure Vessel Technology:;2012:;volume( 134 ):;issue: 005
    contenttypeFulltext
    DSpace software copyright © 2002-2015  DuraSpace
    نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
    yabeshDSpacePersian
     
    DSpace software copyright © 2002-2015  DuraSpace
    نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
    yabeshDSpacePersian