A Criterion for Combination Rule in Flaw Assessment of Parallel Surface CracksSource: Journal of Pressure Vessel Technology:;2011:;volume( 133 ):;issue: 006::page 61204Author:Masayuki Kamaya
DOI: 10.1115/1.4004563Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: When multiple cracks approach one another, the stress intensity factor and J-integral value change due to the interaction of the stress field. Since the changes in these parameters are not always conservative in structural reliability evaluations, the interaction between multiple cracks should be taken into account. Section XI of the ASME Boiler and Pressure Vessel Code provides a flaw characterization rule for interacting multiple cracks. In Section XI, adjacent cracks are replaced with a coalesced single crack when the distance between the cracks is less than half of the crack depth. However, the criterion for the offset distance is given as an absolute value, although the magnitude of the interaction depends on the crack size. In the current study, an alternative criterion for the offset distance was examined. Linear-elastic and elastic–plastic analyses were performed for interacting semicircular and semi-elliptical surface cracks by the finite element method under a tensile or bending load. The change in the stress intensity factors and J-integral values due to the relative spacing of cracks was investigated. Based on the relationship between the magnitude of the interaction and the relative position of the cracks, the allowable ctriterion for the offset distance was discussed.
keyword(s): Stress , Fracture (Materials) , Surface cracks AND Finite element methods ,
|
Collections
Show full item record
| contributor author | Masayuki Kamaya | |
| date accessioned | 2017-05-09T00:46:31Z | |
| date available | 2017-05-09T00:46:31Z | |
| date copyright | December, 2011 | |
| date issued | 2011 | |
| identifier issn | 0094-9930 | |
| identifier other | JPVTAS-28553#061204_1.pdf | |
| identifier uri | http://yetl.yabesh.ir/yetl/handle/yetl/147402 | |
| description abstract | When multiple cracks approach one another, the stress intensity factor and J-integral value change due to the interaction of the stress field. Since the changes in these parameters are not always conservative in structural reliability evaluations, the interaction between multiple cracks should be taken into account. Section XI of the ASME Boiler and Pressure Vessel Code provides a flaw characterization rule for interacting multiple cracks. In Section XI, adjacent cracks are replaced with a coalesced single crack when the distance between the cracks is less than half of the crack depth. However, the criterion for the offset distance is given as an absolute value, although the magnitude of the interaction depends on the crack size. In the current study, an alternative criterion for the offset distance was examined. Linear-elastic and elastic–plastic analyses were performed for interacting semicircular and semi-elliptical surface cracks by the finite element method under a tensile or bending load. The change in the stress intensity factors and J-integral values due to the relative spacing of cracks was investigated. Based on the relationship between the magnitude of the interaction and the relative position of the cracks, the allowable ctriterion for the offset distance was discussed. | |
| publisher | The American Society of Mechanical Engineers (ASME) | |
| title | A Criterion for Combination Rule in Flaw Assessment of Parallel Surface Cracks | |
| type | Journal Paper | |
| journal volume | 133 | |
| journal issue | 6 | |
| journal title | Journal of Pressure Vessel Technology | |
| identifier doi | 10.1115/1.4004563 | |
| journal fristpage | 61204 | |
| identifier eissn | 1528-8978 | |
| keywords | Stress | |
| keywords | Fracture (Materials) | |
| keywords | Surface cracks AND Finite element methods | |
| tree | Journal of Pressure Vessel Technology:;2011:;volume( 133 ):;issue: 006 | |
| contenttype | Fulltext |