YaBeSH Engineering and Technology Library

    • Journals
    • PaperQuest
    • YSE Standards
    • YaBeSH
    • Login
    View Item 
    •   YE&T Library
    • ASME
    • Journal of Fuel Cell Science and Technology
    • View Item
    •   YE&T Library
    • ASME
    • Journal of Fuel Cell Science and Technology
    • View Item
    • All Fields
    • Source Title
    • Year
    • Publisher
    • Title
    • Subject
    • Author
    • DOI
    • ISBN
    Advanced Search
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Archive

    Phase Stability and Sintering Behavior of 10mol%Sc2O3–1mol%CeO2–ZrO2 Ceramics

    Source: Journal of Fuel Cell Science and Technology:;2009:;volume( 006 ):;issue: 002::page 21007
    Author:
    Nicholas Bernier
    ,
    Sergey Yarmolenko
    ,
    Jag Sankar
    ,
    Michael Klimov
    ,
    Jay Kapat
    ,
    Nina Orlovskaya
    DOI: 10.1115/1.2971126
    Publisher: The American Society of Mechanical Engineers (ASME)
    Abstract: The phase composition and sintering behavior of two commercially available 10mol%Sc2O3–1mol%CeO2–ZrO2 ceramics produced by Daiichi Kigenso Kagaku Kogyo (DKKK) and Praxair have been studied. DKKK powders have been manufactured using a wet coprecipitation chemical route, and Praxair powders have been produced by spray pyrolysis. The morphology of the powders, as studied by scanning electron microscopy, has been very different. DKKK powders were presented as soft (∼100μm) spherical agglomerates containing 60–100nm crystalline particles, whereas the Praxair powders were presented as sintered platelet agglomerates, up to 30μm long and 3–4μm thick, which consisted of smaller 100–200nm crystalline particles. X-ray diffraction analysis has shown that both DKKK and Praxair powders contained a mixture of cubic (c) and rhombohedral (r) phases: 79% cubic +21% rhombohedral for DKKK powders and 88% cubic +12% rhombohedral for Praxair powders. Higher quantities of the Si impurity level have been detected in Praxair powder as compared to DKKK powder by secondary ion mass spectroscopy. The morphological features, along with differences in composition and the impurity level of both powders, resulted in significantly different sintering behaviors. The DKKK powders showed a more active sintering behavior than of Praxair powders, reaching 93–95% of theoretical density when sintered at 1300°C for 2h. Comparatively, the Praxair powders required high sintering temperatures at 1500–1600°C. However, even at such high sintering temperatures, a significant amount of porosity was observed. Both DKKK and Praxair ceramics sintered at 1300°C or above exist in a cubic phase at room temperature. However, if sintered at 1100°C and 1200°C, the DKKK ceramics exist in a rhombohedral phase at room temperature. The DKKK ceramics sintered at 1300°C or above exhibit cubic to rhombohedral and back to cubic phase transitions upon heating at a 300–500°C temperature range, while Praxair ceramics exist in a pure cubic phase upon heating from room temperature to 900°C. However, if heated rather fast, the cubic to rhombohedral phase transformation could be avoided. Thus it is not expected that the observed phase transitions play a significant role in developing transformation stresses in ScCeZrO2 electrolyte upon heating and cooling down from the operation temperatures.
    keyword(s): Temperature , Ceramics , Sintering , Zirconium AND Heating ,
    • Download: (1.189Mb)
    • Show Full MetaData Hide Full MetaData
    • Get RIS
    • Item Order
    • Go To Publisher
    • Statistics

      Phase Stability and Sintering Behavior of 10mol%Sc2O3–1mol%CeO2–ZrO2 Ceramics

    URI
    https://yetl.yabesh.ir/yetl1/handle/yetl/140860
    Collections
    • Journal of Fuel Cell Science and Technology

    Show full item record

    contributor authorNicholas Bernier
    contributor authorSergey Yarmolenko
    contributor authorJag Sankar
    contributor authorMichael Klimov
    contributor authorJay Kapat
    contributor authorNina Orlovskaya
    date accessioned2017-05-09T00:33:26Z
    date available2017-05-09T00:33:26Z
    date copyrightMay, 2009
    date issued2009
    identifier issn2381-6872
    identifier otherJFCSAU-28937#021007_1.pdf
    identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/140860
    description abstractThe phase composition and sintering behavior of two commercially available 10mol%Sc2O3–1mol%CeO2–ZrO2 ceramics produced by Daiichi Kigenso Kagaku Kogyo (DKKK) and Praxair have been studied. DKKK powders have been manufactured using a wet coprecipitation chemical route, and Praxair powders have been produced by spray pyrolysis. The morphology of the powders, as studied by scanning electron microscopy, has been very different. DKKK powders were presented as soft (∼100μm) spherical agglomerates containing 60–100nm crystalline particles, whereas the Praxair powders were presented as sintered platelet agglomerates, up to 30μm long and 3–4μm thick, which consisted of smaller 100–200nm crystalline particles. X-ray diffraction analysis has shown that both DKKK and Praxair powders contained a mixture of cubic (c) and rhombohedral (r) phases: 79% cubic +21% rhombohedral for DKKK powders and 88% cubic +12% rhombohedral for Praxair powders. Higher quantities of the Si impurity level have been detected in Praxair powder as compared to DKKK powder by secondary ion mass spectroscopy. The morphological features, along with differences in composition and the impurity level of both powders, resulted in significantly different sintering behaviors. The DKKK powders showed a more active sintering behavior than of Praxair powders, reaching 93–95% of theoretical density when sintered at 1300°C for 2h. Comparatively, the Praxair powders required high sintering temperatures at 1500–1600°C. However, even at such high sintering temperatures, a significant amount of porosity was observed. Both DKKK and Praxair ceramics sintered at 1300°C or above exist in a cubic phase at room temperature. However, if sintered at 1100°C and 1200°C, the DKKK ceramics exist in a rhombohedral phase at room temperature. The DKKK ceramics sintered at 1300°C or above exhibit cubic to rhombohedral and back to cubic phase transitions upon heating at a 300–500°C temperature range, while Praxair ceramics exist in a pure cubic phase upon heating from room temperature to 900°C. However, if heated rather fast, the cubic to rhombohedral phase transformation could be avoided. Thus it is not expected that the observed phase transitions play a significant role in developing transformation stresses in ScCeZrO2 electrolyte upon heating and cooling down from the operation temperatures.
    publisherThe American Society of Mechanical Engineers (ASME)
    titlePhase Stability and Sintering Behavior of 10mol%Sc2O3–1mol%CeO2–ZrO2 Ceramics
    typeJournal Paper
    journal volume6
    journal issue2
    journal titleJournal of Fuel Cell Science and Technology
    identifier doi10.1115/1.2971126
    journal fristpage21007
    identifier eissn2381-6910
    keywordsTemperature
    keywordsCeramics
    keywordsSintering
    keywordsZirconium AND Heating
    treeJournal of Fuel Cell Science and Technology:;2009:;volume( 006 ):;issue: 002
    contenttypeFulltext
    DSpace software copyright © 2002-2015  DuraSpace
    نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
    yabeshDSpacePersian
     
    DSpace software copyright © 2002-2015  DuraSpace
    نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
    yabeshDSpacePersian