dc.description.abstractGas-tungsten-arc weldments in Alloy 718 were studied in fatigue-crack growth tests conducted at five temperatures over the range 24–649°C. In general, crack growth rates increased with increasing temperature, and weldments given the “conventional” post-weld heat-treatment generally exhibited crack growth rates that were higher than for weldments given the “modified” (INEL) heat-treatment. Limited testing in the as-welded condition revealed crack growth rates significantly lower than observed for the heat-treated cases, and this was attributed to residual stresses. Three different heats of filler wire were utilized, and no heat-to-heat variations were noted.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleEffect of Heat-Treatment Upon the Fatigue-Crack Growth Behavior of Alloy 718 Weldments—Part I: Macroscopic Behavior
dc.typeJournal Paper
dc.journal.volume107
dc.journal.issue1
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225768
dc.journal.fristpage34
dc.journal.lastpage40
dc.identifier.eissn1528-8889
dc.keywordsAlloys
dc.keywordsHeat treating (Metalworking)
dc.keywordsFatigue cracks
dc.keywordsFracture (Materials)
dc.keywordsHeat
dc.keywordsTemperature
dc.keywordsTesting
dc.keywordsWire
dc.keywordsFillers (Materials)
dc.keywordsResidual stresses
dc.keywordsIndium alloys AND Tungsten
dc.treeJournal of Engineering Materials and Technology:;1985:;volume( 107 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record