dc.description.abstractFracture toughness tests were performed at 93, 205, 316, and 427°C using electropotential techniques on HT-9 weld material irradiated to a fluence of 2.35 × 1022 n/cm2 (E> 0.1 MeV) at 390°C. Testing of welds irradiated at 450, 500, and 550°C was performed at 205°C. Test results were analyzed using the J-integral approach. It was found that the initiation fracture toughness of these HT-9 welds increased slightly, while the tearing modulus decreased significantly after irradiation to a fluence of 2.35 × 1022 n/cm2 . In addition, results showed that irradiation temperature had little effect on the initiation fracture toughness of HT-9 weld metal. The specimens were examined by scanning electron microscopy after the test in order to understand the fracture process in this weld material.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFracture Toughness of Irradiated HT-9 Weld Metal
dc.typeJournal Paper
dc.journal.volume107
dc.journal.issue4
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225827
dc.journal.fristpage329
dc.journal.lastpage333
dc.identifier.eissn1528-8889
dc.keywordsMetals
dc.keywordsFracture toughness
dc.keywordsIrradiation (Radiation exposure)
dc.keywordsWelded joints
dc.keywordsFluence (Radiation measurement)
dc.keywordsFracture (Process)
dc.keywordsScanning electron microscopy
dc.keywordsTesting AND Temperature
dc.treeJournal of Engineering Materials and Technology:;1985:;volume( 107 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record