Show simple item record

dc.contributor.authorD. A. Scott
dc.contributor.authorG. A. Wolgemuth
dc.contributor.authorJ. A. Aikin
dc.date.accessioned2017-05-08T23:18:41Z
dc.date.available2017-05-08T23:18:41Z
dc.date.copyrightFebruary, 1984
dc.date.issued1984
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28231#104_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/98917
dc.description.abstractTo avoid stress corrosion cracking, a method of producing tube-to-tubesheet joints with low residual stresses was sought. Hydraulic expansion was found to be an acceptable method. In this paper, the experimental and theoretical work done to determine these stresses is presented. The area of interest is the transition region between the expanded and unexpanded sections of tubing. X-ray diffraction, stress corrosion cracking test and strain gaging were the prime measuring techniques used. Extensive use of finite element analysis was also made. In addition, the pull strength, length change, etc., of this type of joint were investigated.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleHydraulically Expanded Tube-to-Tubesheet Joints
dc.typeJournal Paper
dc.journal.volume106
dc.journal.issue1
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3264297
dc.journal.fristpage104
dc.journal.lastpage109
dc.identifier.eissn1528-8978
dc.keywordsGages
dc.keywordsX-ray diffraction
dc.keywordsResidual stresses
dc.keywordsStress corrosion cracking
dc.keywordsStress
dc.keywordsTubing AND Finite element analysis
dc.treeJournal of Pressure Vessel Technology:;1984:;volume( 106 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record