| dc.contributor.author | R. D. Cheverton | |
| dc.contributor.author | D. G. Ball | |
| dc.date.accessioned | 2017-05-08T23:18:36Z | |
| dc.date.available | 2017-05-08T23:18:36Z | |
| dc.date.copyright | November, 1984 | |
| dc.date.issued | 1984 | |
| dc.identifier.issn | 0094-9930 | |
| dc.identifier.other | JPVTAS-28245#375_1.pdf | |
| dc.identifier.uri | http://yetl.yabesh.ir/yetl/handle/yetl/98859 | |
| dc.description.abstract | A continuing analysis of the pressurized-thermal-shock problem associated with PWR postulated overcooling accidents indicates that the previously accepted degree of conservatism in the fracture-mechanics model needs to be more closely evaluated, and, if excessive, reduced. One feature that was believed to be conservative was the use of two-dimensional as opposed to finite-length (three-dimensional) flaws. The degree of conservatism could not be adequately investigated because of computational limitations and a lack of knowledge regarding flaw behavior; however, that situation has changed to the extent that some cases involving finite-length flaws can be studied. A flaw of particular interest is one that is located in an axial weld of a plate-type vessel. For those vessels that suffer relatively high-radiation damage in the welds, the length of the flaw will be no greater than the length of the weld, and recent calculations indicate that a deep flaw of that length (∼2 m) is not effectively infinitely long, contrary to previous thinking. The benefit to be derived from consideration of the 2-m flaw and also a semi-elliptical flaw with length-to-depth ratio of 6/1 was investigated by analyzing several postulated transients. In doing so the sensitivity of the benefit to a specified maximum crack-arrest toughness and to the duration of the transient was investigated. Results of the analysis indicate that for some conditions the benefit in using the 2-m flaw is substantial, but it decreases with increasing pressure, and above a certain pressure there may be no benefit, depending on the duration of the transient and the limit on crack-arrest toughness. | |
| dc.publisher | The American Society of Mechanical Engineers (ASME) | |
| dc.title | A Reassessment of PWR Pressure Vessel Integrity During Overcooling Accidents, Considering 3-D Flaws | |
| dc.type | Journal Paper | |
| dc.journal.volume | 106 | |
| dc.journal.issue | 4 | |
| dc.journal.title | Journal of Pressure Vessel Technology | |
| dc.identifier.doi | 10.1115/1.3264367 | |
| dc.journal.fristpage | 375 | |
| dc.journal.lastpage | 382 | |
| dc.identifier.eissn | 1528-8978 | |
| dc.keywords | Pressure vessels | |
| dc.keywords | Accidents | |
| dc.keywords | Pressurized water reactors | |
| dc.keywords | Fracture (Materials) | |
| dc.keywords | Toughness | |
| dc.keywords | Vessels | |
| dc.keywords | Pressure | |
| dc.keywords | Fracture mechanics | |
| dc.keywords | Radiation (Physics) | |
| dc.keywords | Shock (Mechanics) AND Welded joints | |
| dc.tree | Journal of Pressure Vessel Technology:;1984:;volume( 106 ):;issue: 004 | |