dc.description.abstractOrthogonal machining experiments were conducted at the cutting speed of 8.5 × 10−2 cm/s with 6061-T6 aluminum, 4340 steel and Ti-6Al-4V titanium to measure strain distributions in the deformed chip using a grid analysis technique. While the aluminum alloy with low strength and the steel with high strain hardening coefficient displayed large uniform strains with a continuous chip morphology, the titanium alloy exhibited highly nonuniform strain distributions within segmented chips. Some of these observations as well as published machining test results could be rationalized on the basis of a shear failure criterion where a specific level of critical shear strain might be estimated on the basis of a thermal-mechanical instability analysis.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleThe Nature of Chip Formation in Orthogonal Machining
dc.typeJournal Paper
dc.journal.volume106
dc.journal.issue1
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225683
dc.journal.fristpage9
dc.journal.lastpage15
dc.identifier.eissn1528-8889
dc.keywordsMachining
dc.keywordsSteel
dc.keywordsShear (Mechanics)
dc.keywordsCutting
dc.keywordsFailure
dc.keywordsTitanium
dc.keywordsWork hardening
dc.keywordsAluminum alloys
dc.keywordsTitanium alloys AND Aluminum
dc.treeJournal of Engineering Materials and Technology:;1984:;volume( 106 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record