dc.description.abstractIntergranular cavitation may be a limiting factor in the otherwise highly promising commercial exploitation of the recently developed superplastic forming process for the high strength aluminum alloy, 7475. A preliminary investigation has been carried out to quantify the effects of superplastic deformation on the major ambient temperature service properties. It is shown that the properties most degraded by the development of cavitation after large superplastic strains are those that depend on the local strain at tensile fracture. This affects, mainly, ductility and fatigue life. However, the effects are not generally significant below effective superplastic strains of about 0.8 to 0.9 (120–150 percent elongation) with the optimum forming conditions (T=516°C, ε̇=2×10−4 s−1 ). Furthermore, since the fine grain processing has an initial beneficial effect on the ductility-related properties, compared to conventionally processed sheet, most superplastically formed components would suffer very litle, if any, design penalties.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleThe Effect of Superplastic Deformation on Subsequent Service Properties of Fine Grained 7475 Al
dc.typeJournal Paper
dc.journal.volume105
dc.journal.issue1
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225619
dc.journal.fristpage55
dc.journal.lastpage60
dc.identifier.eissn1528-8889
dc.keywordsDeformation
dc.keywordsSuperplasticity
dc.keywordsCavitation
dc.keywordsDuctility
dc.keywordsDesign
dc.keywordsFracture (Process)
dc.keywordsElongation
dc.keywordsFatigue life
dc.keywordsSuperplastic forming
dc.keywordsTemperature AND Aluminum alloys
dc.treeJournal of Engineering Materials and Technology:;1983:;volume( 105 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record