dc.description.abstractIt is well known that fracture initiation behavior is influenced by weld thermal straining. In the present report, attention is focused on the influence of weld thermal straining on the fracture mechanism. The influence of prestrain at elevated temperature or strain-aging on the initiation and propagation behaviors of ductile and cleavage fracture in KD32 and HT80 steels is investigated. A relationship between the increase in the lowest temperature at which a tear dimple region can be observed (Ti ) or the decrease in stretched zone width and the increase in hardness at the notch tip is found.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleEffect of Prestrain at Elevated Temperature on the Fracture Behavior of High Strength Steels
dc.typeJournal Paper
dc.journal.volume105
dc.journal.issue1
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225612
dc.journal.fristpage16
dc.journal.lastpage20
dc.identifier.eissn1528-8889
dc.keywordsTemperature
dc.keywordsSteel
dc.keywordsFracture (Process) AND Mechanisms
dc.treeJournal of Engineering Materials and Technology:;1983:;volume( 105 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record