dc.description.abstractBasic damage tolerance properties of Ti-6Al-4V titanium plate can be improved by laminating thin sheets of titanium with adhesives. Compact tension and center-cracked tension specimens made from thick plate, thin sheet, and laminated plate (six plies of thin sheet) were tested. The fracture toughness of the laminated plate was 39 percent higher than the monolithic plate. The laminated plate’s through-the-thickness crack growth rate was about 20 percent less than that of the monolithic plate. The damage tolerance life of the surface-cracked laminate was 6 to over 15 times the life of a monolithic specimen.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleDamage Tolerance Evaluation of Adhesively Laminated Titanium
dc.typeJournal Paper
dc.journal.volume105
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225641
dc.journal.fristpage182
dc.journal.lastpage187
dc.identifier.eissn1528-8889
dc.keywordsTitanium
dc.keywordsTension
dc.keywordsThickness
dc.keywordsAdhesives
dc.keywordsLaminates
dc.keywordsFracture (Materials) AND Fracture toughness
dc.treeJournal of Engineering Materials and Technology:;1983:;volume( 105 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record