dc.description.abstractOxygen-free copper, 6061 aluminum, and 1100 aluminum bars were drawn from various initial diameters in the annealed state to bars of 11.8 mm (0.464 in.) at maximum reductions in area up to 79.5 percent. It was found that an apparent lack of hardening existed at the higher strains up to the maximum investigated as was determined in tension tests of the drawn bars. The lack of hardening observed was thought to be due, at least in part, to the development of microcracks at the larger strains, a theory proposed by Shaw. It was also found that the oxygen-free copper of the two different heats had appreciable variations in ductility at fracture in tension tests. The reason for this behavior was not determined.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleLack of Hardening in Drawn Bars of Copper and Aluminum in Tension Tests
dc.typeJournal Paper
dc.journal.volume104
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225069
dc.journal.fristpage227
dc.journal.lastpage233
dc.identifier.eissn1528-8889
dc.keywordsCopper
dc.keywordsAluminum
dc.keywordsHardening
dc.keywordsTension
dc.keywordsOxygen
dc.keywordsDuctility
dc.keywordsFracture (Process) AND Microcracks
dc.treeJournal of Engineering Materials and Technology:;1982:;volume( 104 ):;issue: 003