dc.description.abstractAn attempt is made to rationalize the fracture behavior of pearlitic gray irons on both the microstructural and macrostructural levels. Along with the effects of inoculation, those of as-cast section size and carbon equivalent may be rationalized on the basis of coarseness and volume fraction of the weak graphite flakes present in the structure based upon Hornbogen and Motz microstructural model. On the macrostructural level, however, the eutectic cell size is the single most important parameter controlling fracture behavior of gray irons. An analytical model is developed to predict the fracture toughness as a function of notched tensile strength and eutectic cell size. Analytical predictions on both the microstructural and macrostructural levels compare well with experimental results.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleMicrostructural and Macrostructural Modeling of the Fracture Behavior of Pearlitic Gray Irons
dc.typeJournal Paper
dc.journal.volume104
dc.journal.issue4
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225074
dc.journal.fristpage262
dc.journal.lastpage266
dc.identifier.eissn1528-8889
dc.keywordsFracture (Process)
dc.keywordsModeling
dc.keywordsIrons (Textile pressing)
dc.keywordsCarbon
dc.keywordsFracture toughness
dc.keywordsGraphite AND Tensile strength
dc.treeJournal of Engineering Materials and Technology:;1982:;volume( 104 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record