dc.description.abstractA hydrogen-induced fracture process in the HAZ of a QT-steel weldment is studied numerically. Two-dimensional models are used to estimate the transient distributions of stress and hydrogen during the cooling and during the subsequent crack propagation. The distributions of hydrogen in front of a blunted crack are studied for different void volumes in the fracture zone corresponding to brittle and ductile fracture mechanisms. It is tentatively concluded that the incubation time at slow crack growth is not controlled by the hydrostatic stress. A ductile fracture mechanism leading to a relative void volume of 0.02-0.05 in the fracture zone is found to imply long incubation times resulting in a low average crack propagation speed.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleHydrogen-Induced Crack Propagation in a QT-Steel Weldment
dc.typeJournal Paper
dc.journal.volume104
dc.journal.issue4
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225072
dc.journal.fristpage249
dc.journal.lastpage256
dc.identifier.eissn1528-8889
dc.keywordsSteel
dc.keywordsCrack propagation
dc.keywordsHydrogen
dc.keywordsFracture (Process)
dc.keywordsStress
dc.keywordsDuctile fracture
dc.keywordsMechanisms
dc.keywordsBrittleness
dc.keywordsHydrostatics AND Cooling
dc.treeJournal of Engineering Materials and Technology:;1982:;volume( 104 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record