dc.description.abstractThe paper deals with the development of control-rolled Cu-Ni-Cb HSLA steels with increased section capability for low-temperature environments and Cu-Ti-B HSLA steels for general structural applications as well as for specialized applications requiring quench and temper treatments. Results indicate that based on 2 percent copper additions it is possible to develop HSLA steels with strength level of over 690 MPa with sufficiently low transition temperatures (−40°C to lower than −70°C) and very upper shelf values (170 J to 270 J). In the boron-containing compositions, even in the absence of nickel, strength levels of 480 to 820 MPa with a T. T. of −20°C to lower than −60°C have been realized depending upon the rolling practice and the reheat and quench practice. The practical implications of the study are discussed.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleStrong Tough HSLA Steels Via Processing and Heat Treating of Cu-Ni-Cb and Cu-Ti-B Compositions
dc.typeJournal Paper
dc.journal.volume103
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225002
dc.journal.fristpage207
dc.journal.lastpage211
dc.identifier.eissn1528-8889
dc.keywordsHeat
dc.keywordsSteel
dc.keywordsToughness
dc.keywordsPhase transition temperature
dc.keywordsLow temperature
dc.keywordsCopper AND Nickel
dc.treeJournal of Engineering Materials and Technology:;1981:;volume( 103 ):;issue: 003