Show simple item record

dc.contributor.authorL. A. Simpson
dc.date.accessioned2017-05-08T23:08:56Z
dc.date.available2017-05-08T23:08:56Z
dc.date.copyrightJanuary, 1980
dc.date.issued1980
dc.identifier.issn0094-4289
dc.identifier.otherJEMTA8-26874#97_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/93404
dc.description.abstractCrack opening displacement (COD) has been determined in Zr-2.5 percent Nb over a wide range of applied stress intensity, K. Prior to initiation of crack extension, COD was determined from measurements of stretch zones in specimens which had undergone hydrogen-induced, sub-critical crack growth. In post initiation measurements (during slow stable crack extension), COD was determined from crack face displacement. Both methods were self consistent and depended on the plastic-zone-corrected K in accordance with the Wells equation. The J-integral was also determined during stable crack extension using the method of Garwood, et al. The results are consistent with the COD measurements based on theoretical relationships between the two crack tip parameters.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleThe Relationship Between Stress Intensity Factor, Crack Opening Displacement and J-Integral in Zr-2.5 Percent Nb
dc.typeJournal Paper
dc.journal.volume102
dc.journal.issue1
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3224792
dc.journal.fristpage97
dc.journal.lastpage100
dc.identifier.eissn1528-8889
dc.keywordsStress
dc.keywordsFracture (Materials)
dc.keywordsDisplacement
dc.keywordsZirconium
dc.keywordsMeasurement
dc.keywordsWells
dc.keywordsEquations AND Hydrogen
dc.treeJournal of Engineering Materials and Technology:;1980:;volume( 102 ):;issue: 001