dc.description.abstractSome failure experiences with metallic components at the Synthane coal-gasification pilot plant are presented. In some cases, corrosion caused by a sulfur environment was a major factor in the failure initiation. Several instances of improper component manufacture or heat treatment led to failures. Chloride-assisted stress-corrosion cracking and an improper materials choice contributed to two cases of failure. In most cases, the recommended changes in materials, design or process conditions have resulted in an increase in component life.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleMaterials Problems Experienced at the Synthane Coal-Gasification Pilot Plant
dc.typeJournal Paper
dc.journal.volume101
dc.journal.issue2
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3443660
dc.journal.fristpage105
dc.journal.lastpage113
dc.identifier.eissn1528-8889
dc.keywordsCoal
dc.keywordsFuel gasification
dc.keywordsIndustrial plants
dc.keywordsFailure
dc.keywordsSulfur
dc.keywordsStress corrosion cracking
dc.keywordsHeat treating (Metalworking)
dc.keywordsCorrosion
dc.keywordsDesign AND Fracture (Process)
dc.treeJournal of Engineering Materials and Technology:;1979:;volume( 101 ):;issue: 002
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record