dc.description.abstractIn a fusion reactor, various parts will be exposed to an important flux of helium atoms. Under certain conditions this will cause blistering resulting in surface erosion and plasma contamination. We discuss measurements of the following blister parameters: blister skin structure and thickness, helium depth distribution, and swelling. These data refer mainly to 10-20 ke V He blistering of Nb and Cu where the blister skin is apparently two times thicker than in the “gas pressure” model. However, the observation of a depletion at the center of the helium distribution, of bubbles in the skin, and of ∼ 40 percent swelling allow us to conclude that this model is still valid.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleHelium Blistering in Metals
dc.typeJournal Paper
dc.journal.volume100
dc.journal.issue4
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3443512
dc.journal.fristpage411
dc.journal.lastpage415
dc.identifier.eissn1528-8889
dc.keywordsMetals AND Helium
dc.treeJournal of Engineering Materials and Technology:;1978:;volume( 100 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record