dc.description.abstractThe performance of several austenitic alloys ranging from low alloy content stainless steels to nickel-base alloys has been evaluated at temperatures from 704–1093°C (1300–2000°F) in cyclic air + 10 percent water vapor and from 704–982°C (1300–1800°F) in gasoline engine exhaust. The gasoline engine exhaust was found to be the more aggresive of the two test environments. A general trend of increasing performance with increasing nickel content was observed. At the highest test temperatures in both tests, the nickel-base alloys clearly displayed superior performance.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleCorrosion Performance of Austenitic Alloys in Automobile Exhaust Environments
dc.typeJournal Paper
dc.journal.volume99
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3443525
dc.journal.fristpage234
dc.journal.lastpage238
dc.identifier.eissn1528-8889
dc.keywordsAlloys
dc.keywordsCorrosion
dc.keywordsAutomobiles
dc.keywordsExhaust systems
dc.keywordsNickel
dc.keywordsGasoline engines
dc.keywordsTemperature
dc.keywordsWater vapor AND Stainless steel
dc.treeJournal of Engineering Materials and Technology:;1977:;volume( 099 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record