dc.description.abstractA series of advanced investigations on the radiation performance of four 6-in-thick plates from a large (30-ton) commercial melt of A533-B steel is described. The melt represented the first commercial scale demonstration test of improved radiation embrittlement resistance through the control (minimization) of selected residual impurity elements. Melt specifications emphasized the attainment of a low copper and phosphorus content; one half of the melt was modified, however, by a copper addition (0.03 percent Cu increased to 0.13 percent Cu). Initial plate tests described superior 550 F (288 C) radiation resistance, in terms of notch ductility retention, for the primary melt composition and verified the detrimental influence of impurity copper on irradiation behavior. Promising capability of the primary melt composition for very high fluence (∼2.5 × 1020 n/cm2 > 1 MeV) service is shown by the current investigations. In addition, a significant influence of copper content on radiation resistance is revealed for a broad range of exposure temperatures. A dependence of 650 F (343 C) postirradiation heat treatment response (notch ductility recovery) on copper content was also found. Charpy-V versus dynamic tear test performance and tensile strength trends with temperature are examined for low (<450 F, 121 C) and elevated (550 to 585 F, 288 to 307 C) temperature irradiation conditions.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFurther Observations on A533-B Steel Plate Tailored for Improved Radiation Embrittlement Resistance
dc.typeJournal Paper
dc.journal.volume98
dc.journal.issue2
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3454347
dc.journal.fristpage111
dc.journal.lastpage117
dc.identifier.eissn1528-8978
dc.keywordsSteel
dc.keywordsRadiation (Physics)
dc.keywordsElectrical resistance
dc.keywordsEmbrittlement
dc.keywordsCopper
dc.keywordsTemperature
dc.keywordsDuctility
dc.keywordsIrradiation (Radiation exposure)
dc.keywordsHeat treating (Metalworking)
dc.keywordsFluence (Radiation measurement)
dc.keywordsPlates (structures) AND Tensile strength
dc.treeJournal of Pressure Vessel Technology:;1976:;volume( 098 ):;issue: 002
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record