dc.description.abstractThree-point bend tests were conducted to examine the geometry dependence of JIc in two intermediate-strength aluminum alloys, 2024-T351 and 7005-T6351. The amounts of crack growth at selected points on the load-versus-deflection curves were delineated using a heat tinting technique. Resistance curves of J-versus-crack extension were constructed to facilitate determination of JIc at incipient crack movement. The through-thickness variation in fracture toughness of a 7.6-cm-thick plate of 7005 aluminum was determined and correlated with fractographic and metallographic observations. The current JIc measurements from subsized specimens of 7005 aluminum are compared with previous KIc characterizations using linear-elastic, full-thickness specimens.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleInitial Crack Extension in Two Intermediate-Strength Aluminum Alloys
dc.typeJournal Paper
dc.journal.volume98
dc.journal.issue2
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3443358
dc.journal.fristpage152
dc.journal.lastpage158
dc.identifier.eissn1528-8889
dc.keywordsAluminum alloys
dc.keywordsFracture (Materials)
dc.keywordsAluminum
dc.keywordsThickness
dc.keywordsHeat
dc.keywordsMeasurement
dc.keywordsElectrical resistance
dc.keywordsStress
dc.keywordsDeflection
dc.keywordsFracture toughness AND Geometry
dc.treeJournal of Engineering Materials and Technology:;1976:;volume( 098 ):;issue: 002
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record