| dc.contributor.author | R. L. Klueh | |
| dc.contributor.author | R. E. Oakes | |
| dc.date.accessioned | 2017-05-08T23:00:42Z | |
| dc.date.available | 2017-05-08T23:00:42Z | |
| dc.date.copyright | October, 1976 | |
| dc.date.issued | 1976 | |
| dc.identifier.issn | 0094-4289 | |
| dc.identifier.other | JEMTA8-26848#361_1.pdf | |
| dc.identifier.uri | http://yetl.yabesh.ir/yetl/handle/yetl/88641 | |
| dc.description.abstract | The high strain rate tensile properties of annealed 2 1/4 Cr-1 Mo steel were determined and the tensile behavior from 25 to 566°C and strain rates of 2.67 × 10−6 to 144/s were described. Above 0.1/s at 25°C, both the yield stress and the ultimate tensile strength increased rapidly with increasing strain rate. As the temperature was increased, a dynamic strain aging peak appeared in the ultimate tensile strength-temperature curves. The peak height was a maximum at about 350°C and 2.67 × 10−6 /s. With increasing strain rate, a peak of decreased height occurred at progressively higher temperatures. The major effect of strain rate on ductility occurred at elevated temperatures, where a decrease in strain rate caused an increase in total elongation and reduction in area. | |
| dc.publisher | The American Society of Mechanical Engineers (ASME) | |
| dc.title | High Strain Rate Tensile Properties of Annealed 2 1/4 Cr-1 Mo Steel | |
| dc.type | Journal Paper | |
| dc.journal.volume | 98 | |
| dc.journal.issue | 4 | |
| dc.journal.title | Journal of Engineering Materials and Technology | |
| dc.identifier.doi | 10.1115/1.3443390 | |
| dc.journal.fristpage | 361 | |
| dc.journal.lastpage | 368 | |
| dc.identifier.eissn | 1528-8889 | |
| dc.keywords | Steel | |
| dc.keywords | Temperature | |
| dc.keywords | Ductility | |
| dc.keywords | Elongation | |
| dc.keywords | Tensile strength AND Yield stress | |
| dc.tree | Journal of Engineering Materials and Technology:;1976:;volume( 098 ):;issue: 004 | |
| dc.contenttype | Fulltext | |