Show simple item record

dc.contributor.authorC. A. Griffis
dc.date.accessioned2017-05-08T22:59:35Z
dc.date.available2017-05-08T22:59:35Z
dc.date.copyrightNovember, 1975
dc.date.issued1975
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28122#278_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/87992
dc.description.abstractThe geometry dependence of the J-integral and crack opening displacement at fracture initiation, Ji and (COD)i , is examined for HY-80 steel using precracked bend specimens having thicknesses ranging from 1.6 to 53mm. The amount of crack growth at selected points on the load-deflection diagram was delineated using an unload-heat tint procedure. Resistance curves of J and COD versus crack extension were constructed to determine critical values of these parameters at incipient crack movement. Results are interpreted in terms of previously proposed minimum size requirements for valid Ji measurement. The adequacy of the Rice-Srawley J-integral formula for the bend specimen and the utility of J and COD values at maximum load are also considered.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleElastic-Plastic Fracture Toughness: A Comparison of J-Integral and Crack Opening Displacement Characterizations
dc.typeJournal Paper
dc.journal.volume97
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3454308
dc.journal.fristpage278
dc.journal.lastpage283
dc.identifier.eissn1528-8978
dc.keywordsFracture (Materials)
dc.keywordsDisplacement
dc.keywordsFracture toughness
dc.keywordsStress
dc.keywordsGeometry
dc.keywordsFormulas
dc.keywordsFracture (Process)
dc.keywordsDeflection
dc.keywordsHeat
dc.keywordsSteel AND Electrical resistance
dc.treeJournal of Pressure Vessel Technology:;1975:;volume( 097 ):;issue: 004