dc.contributor.authorJ. O. Stiegler
dc.contributor.authorR. T. King
dc.contributor.authorG. M. Goodwin
dc.date.accessioned2017-05-08T22:58:42Z
dc.date.available2017-05-08T22:58:42Z
dc.date.copyrightJuly, 1975
dc.date.issued1975
dc.identifier.issn0094-4289
dc.identifier.otherJEMTA8-26841#245_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/87516
dc.description.abstractPrevious studies had shown that conventional type 308 stainless steel weld metal can have low creep ductility (< 1 percent total elongation) at 650 deg C. This paper demonstrates that the low ductility results from internal cracks that develop at austenite-sigma phase boundaries and propagate under the test conditions. The sigma phase is formed from ferrite present in the as-deposited weld metal. Type 308 stainless steel weld metal containing controlled amounts of the residual elements B, P, and Ti also contains sigma phase, but phase boundary cracking has not been observed even after 5000 hr. The controlled residual element weld metal is significantly more ductile (> 10 percent total elongation) than the conventional weld metals for which data are available.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleEffect of Residual Elements on Fracture Characteristics and Creep Ductility of Type 308 Stainless Steel Weld Metal
dc.typeJournal Paper
dc.journal.volume97
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3443291
dc.journal.fristpage245
dc.journal.lastpage250
dc.identifier.eissn1528-8889
dc.keywordsCreep
dc.keywordsMetals
dc.keywordsDuctility
dc.keywordsFracture (Process)
dc.keywordsStainless steel
dc.keywordsElongation
dc.keywordsFracture (Materials) AND Ferrites (Magnetic materials)
dc.treeJournal of Engineering Materials and Technology:;1975:;volume( 097 ):;issue: 003
dc.contenttypeFulltext