Show simple item record

dc.contributor.authorKaoru Hasebe
dc.contributor.authorSeizou Usuki
dc.date.accessioned2017-05-08T22:24:34Z
dc.date.available2017-05-08T22:24:34Z
dc.date.copyrightApril 1989
dc.date.issued1989
dc.identifier.other%28asce%290733-9399%281989%29115%3A4%28867%29.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/79997
dc.description.abstractThe failure criterion for orthotropic materials as wood is presented. Using Tsai and Wu criterion the failure criterion for wood is derived under plane stress conditions ignoring the influence of stress perpendicular to the grain. The failure criterion for wood is given by an ellipse. Tests of mechanical properties of Japanese cedar are carried out, where eight groups of wood transmission poles are used. Tests are performed on 104 small specimens to determine direct compressive, tensile and shearing strengtjh of the test materials. The ultimate tensile strength parallel to the grain of the test specimens are 1.5 to 2.4 times the ultimate compressive strength parallel to the grain. The failure criterion for the test specimens is shown.
dc.publisherAmerican Society of Civil Engineers
dc.titleApplication of Orthotropic Failure Criterion to Wood
dc.typeJournal Paper
dc.journal.volume115
dc.journal.issue4
dc.journal.titleJournal of Engineering Mechanics
dc.identifier.doi10.1061/(ASCE)0733-9399(1989)115:4(867)
dc.treeJournal of Engineering Mechanics:;1989:;Volume ( 115 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record