dc.description.abstractForty-five glass fiber reinforced polymer (GFRP) rebars were tested in compression to determine their ultimate strength and Young’s modulus. The rebars (or C-bars), produced by Marshall Industries Composites, Inc., had an outside diameter of 15 mm (#15 rebar), and unbraced lengths varying from 50 to 380 mm. A compression test method was developed to conduct the experiments. Three failure modes, that are directly related to the unbraced length of the rebar, are identified as crushing, buckling, and combined buckling and crushing. The crushing region represents the failure mode a GFRP rebar would experience when confined in concrete under compression. The experimental results showed that the ultimate compressive strength of the #15 GFRP rebar failing by crushing is approximately 50% of the ultimate tensile strength. Based on a very limited number of tests, in which strain readings were acceptable, Young’s modulus in compression was found to be approximately the same as in tension.
dc.publisherAmerican Society of Civil Engineers
dc.titlePhysical Properties of Glass Fiber Reinforced Polymer Rebars in Compression
dc.typeJournal Paper
dc.journal.volume7
dc.journal.issue4
dc.journal.titleJournal of Composites for Construction
dc.identifier.doi10.1061/(ASCE)1090-0268(2003)7:4(363)
dc.treeJournal of Composites for Construction:;2003:;Volume ( 007 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record