dc.description.abstractAccelerated aging tests are being conducted on more than 20 types of glass fiber-reinforced polymer (GFRP) reinforcing bars, which are produced from different combinations of constituent materials, manufacturing parameters, sizes and shapes, and surface coatings. The specimens are being subjected to various sustained tensile loading (22 to 68% of ultimate strength) in three types of alkaline environments: NaOH, simulated pore-water solution, and embedded in concrete. Time to rupture or residual strength, as applicable, have been determined. Additionally, stress corrosion mechanisms were evaluated by various microstructural analyses. The results showed clearly that alkaline ions and moisture could penetrate or diffuse through the resin (or through cracks and voids) to the interphases and the fibers. For GFRP bars embedded in moist concrete under various sustained stress levels, three types of stress corrosion mechanisms have been identified: stress dominated, crack propagation dominated, and diffusion dominated.
dc.publisherAmerican Society of Civil Engineers
dc.titleDurability of Glass Fiber-Reinforced Polymer Reinforcing Bars in Concrete Environment
dc.typeJournal Paper
dc.journal.volume6
dc.journal.issue3
dc.journal.titleJournal of Composites for Construction
dc.identifier.doi10.1061/(ASCE)1090-0268(2002)6:3(143)
dc.treeJournal of Composites for Construction:;2002:;Volume ( 006 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record