dc.contributor.authorHe, Jiechen
dc.contributor.authorTian, Wenshan
dc.contributor.authorGong, Youjing
dc.contributor.authorDuan, Kaijiao
dc.contributor.authorLiu, Tiancheng
dc.date.accessioned2026-08-20T11:54:08Z
dc.date.available2026-08-20T11:54:08Z
dc.date.copyright2025/06/27
dc.date.issued2025
dc.identifier.otherJOEEDU.EEENG-8183.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl1/handle/yetl/4312821
dc.description.abstractAbstractThe MgO/ZrO2 catalyst was prepared using the solvothermal method for NO catalytic oxidation. The MgO/ZrO2 catalyst was modified by adding polyvinylpyrro-lidone (PVP) and polyethylene glycol-2000 (PEG-2000) template agents, and different template pairs were ...
dc.publisherAmerican Society of Civil Engineers
dc.titleEffect of Template Agent on Catalytic Oxidation of NO by MgO/ZrO2
dc.typeJournal Article
dc.journal.volume151
dc.journal.issue9
dc.journal.titleJournal of Environmental Engineering
dc.identifier.doi10.1061/JOEEDU.EEENG-8183
dc.journal.fristpage04025048-1
dc.journal.lastpage04025048-9
dc.page9
dc.treeJournal of Environmental Engineering:;2025:;Volume ( 151 ):;issue: 009