Show simple item record

dc.contributor.authorGarakani, Behnam
dc.contributor.authorSomarathna, Udara S.
dc.contributor.authorUmar, Ashraf
dc.contributor.authorKhinda, Gurvinder Singh
dc.contributor.authorAbdelatty, Mohamed Youssef M.
dc.contributor.authorAbbara, El Mehdi
dc.contributor.authorAl Zerey, Sari
dc.contributor.authorHopkins, Mike
dc.contributor.authorSrinivas, Sai
dc.contributor.authorKinzel, Chuck
dc.contributor.authorHalseth, Christopher
dc.contributor.authorRonay, Mark
dc.contributor.authorPoliks, Mark D.
dc.date.accessioned2023-08-16T18:15:15Z
dc.date.available2023-08-16T18:15:15Z
dc.date.copyright2/1/2023 12:00:00 AM
dc.date.issued2023
dc.identifier.issn1043-7398
dc.identifier.otherep_145_03_031006.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl1/handle/yetl/4291713
dc.description.abstractLiquid metal-based gallium conductors exhibit unique physical and electromechanical properties, which make them excellent candidates for the next generation of wearable electronics. In this study, a novel fluid phase-based gallium conductor was stencil printed on thermoplastic polyurethane (TPU) to fabricate a stretchable conductor as well as a stretchable radio frequency (RF) transmission line. The electromechanical reliability of the conductor during high elongation as well as cyclic tension and bend fatigue was evaluated and compared with commercially available stretchable silver-filled polymer paste. The microstructure of the liquid metal conductor and the silver paste was investigated via scanning electron microscopy (SEM) before and after the samples were subjected to high elongation (>100%). Unlike the silver paste, the liquid metal conductor maintained its microstructural integrity while its resistance showed a linear response to changes in length. A cyclic tension fatigue test confirmed the fatigue-free performance of the liquid metal conductor during 8000 stretching cycles at a strain amplitude of 30%. The electromagnetic structure of the RF transmission line was simulated and then compared to the measured data. The measurements for insertion loss showed that U-bending, 90 deg twisting, and 1000 stretching cycles at a strain amplitude of 100% did not have a significant impact on the RF performance. Details of the DC tests and RF measurements, including the microstructural analysis and simulation results, will be discussed in this article.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleInvestigation of Electromechanical Reliability and Radio Frequency Performance of a Highly Stretchable Liquid Metal Conductor for Wearable Electronics
dc.typeJournal Paper
dc.journal.volume145
dc.journal.issue3
dc.journal.titleJournal of Electronic Packaging
dc.identifier.doi10.1115/1.4056640
dc.journal.fristpage31006-1
dc.journal.lastpage31006-11
dc.page11
dc.treeJournal of Electronic Packaging:;2023:;volume( 145 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record