dc.description.abstractIn this paper, a new controlling method combined local postweld heat treatment (PWHT) and water jet peening (WJP) was proposed to reduce full-field residual stress of girth weld with thick wall. The finite element analysis with sequential coupling method and experiment measurement were performed to study the residual stresses distribution before and after the new controlling method. The results show that the hoop and axial stresses through the thickness are all decreased greatly by using the new controlling method. As long as the new controlling method is used with appropriate parameters, the residual stresses on inner surface can be reduced from tensile stresses to compressive stresses, which greatly improve the resistance ability to stress corrosion of inner surface.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleReducing Full-Field Residual Stress of Girth Weld With Thick Wall by Combining Local PWHT and Water Jet Peening
dc.typeJournal Paper
dc.journal.volume144
dc.journal.issue6
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4054301
dc.journal.fristpage61302-1
dc.journal.lastpage61302-8
dc.page8
dc.treeJournal of Pressure Vessel Technology:;2022:;volume( 144 ):;issue: 006
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record