    Performance Degradation and Poison Build-Up of an Oxidation Catalyst in Two-Stroke Natural Gas Engine Exhaust

    Thumbnail
    View/Open
    jert_140_07_072208.pdf (3.079Mb)
    Date
    2018
    Author
    Baumgardner, Marc E.
    Olsen, Daniel B.
    Metadata
    Show full item record
    Abstract
    Due to current and future exhaust emissions regulations, oxidation catalysts are increasingly being added to the exhaust streams of large-bore, two-stroke, natural gas engines. Such catalysts have a limited operational lifetime, primarily due to chemical (i.e., catalyst poisoning) and mechanical fouling resulting from the carry-over of lubrication oil from the cylinders. It is critical for users and catalyst developers to understand the nature and rate of catalyst deactivation under these circumstances. This study examines the degradation of an exhaust oxidation catalyst on a large-bore, two-stroke, lean-burn, natural gas field engine over the course of 2 years. Specifically, this work examines the process by which the catalyst was aged and tested and presents a timeline of catalyst degradation under commercially relevant circumstances. The catalyst was aged in the field for 2-month intervals in the exhaust slipstream of a GMVH-12 engine and intermittently brought back to Colorado State University for both engine testing and catalyst surface analysis. Engine testing consisted of measuring catalyst reduction efficiency as a function of temperature as well as the determination of the light-off temperature for several exhaust components. The catalyst surface was analyzed via scanning electron microscope (SEM)/energy dispersive X-ray spectroscopy (EDS) and X-ray photoelectron spectroscopy (XPS) techniques to examine the location and rate of poison deposition. After 2 years online, the catalyst light-off temperature had increased ∼55 °F (31 °C) and ∼34 wt % poisons (S, P, Zn) were built up on the catalyst surface, both of which represent significant catalyst deactivation.
    URI
    http://yetl.yabesh.ir/yetl1/handle/yetl/4254212
    Collections
    • Journal of Energy Resources Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV