dc.description.abstractThe American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-versus-life (ε–N) data illustrate significant effects of LWR water environments on the fatigue resistance of pressure vessel and piping steels. Extensive studies have been conducted at Argonne National Laboratory (Argonne) and elsewhere to investigate the effects of LWR environments on the fatigue life. This article summarizes the results of these studies. The existing fatigue ε–N data were evaluated to identify the various material, environmental, and loading conditions that influence the fatigue crack initiation; a methodology for estimating fatigue lives as a function of these parameters was developed. The effects were incorporated into the ASME Code Section III fatigue evaluations in terms of an environmental correction factor, Fen, which is the ratio of fatigue life in air at room temperature to the life in the LWR water environment at reactor operating temperatures. Available fatigue data were used to develop fatigue design curves for carbon and low-alloy steels, austenitic stainless steels (SSs), and nickel–chromium–iron (Ni–Cr–Fe) alloys and their weld metals. A review of the Code Section III fatigue adjustment factors of 2 and 20 is also presented, and the possible conservatism inherent in the choice is evaluated. A brief description of potential effects of neutron irradiation on fatigue crack initiation is presented.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleEffect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials
dc.typeJournal Paper
dc.journal.volume139
dc.journal.issue6
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4035885
dc.journal.fristpage60801
dc.journal.lastpage060801-21
dc.treeJournal of Pressure Vessel Technology:;2017:;volume( 139 ):;issue: 006
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record