    The Effects of the Material's Exact Yield Point and Its Plastic Properties on the Safe Maximum Pressure of Gun Barrels

    Thumbnail
    View/Open
    pvt_139_05_051401.pdf (1.456Mb)
    Date
    2017
    Author
    Perry, J.
    Perl, M.
    Metadata
    Show full item record
    Abstract
    The design of a gun barrel aims at maximizing its firing power, determined by its safe maximum pressure (SMP)—the maximal allowed firing pressure—which is considerably enhanced by inducing a favorable residual stress field through the barrel's wall commonly by the autofrettage process. Presently, there are two distinct processes: hydrostatic and swage autofrettage. In both processes, the barrel's material is fully or partially plastically deformed. Recently, a 3D computer code has been developed, which finally enables a realistic simulation of both swage and hydraulic autofrettage processes, using the experimentally measured stress–strain curve and incorporating the Bauschinger effect. This code enables a detailed analysis of all the factors relating to the final SMP of a barrel and can be used to establish the optimal process for any gun-barrel design. A major outcome of this analysis was the fact that the SMP of an autofrettaged barrel is dictated by the detailed plastic characteristics on the barrel's material. The main five plastic parameters of the material that have been identified are: the exact (zero offset) value of the yield stress, the universal plastic curve in both tension and compression, the Bauschinger effect factor (BEF) curve, and the elastic–plastic transition range (EPTR). A detailed comparison between three similar barrel materials points to the fact that the major parameter determining the barrel's SMP is the yield stress of the material and that the best way to determine it is by the newly developed “zero offset” method. All other four parameters are found to have a greater influence on the SMP of a hydraulically autofrettaged barrel than on a swaged one. The simplicity of determining the zero offset yield stress will enable its use in any common elastic and elastoplastic problem instead of the present 0.1% or 0.2% yield stress methods.
    URI
    http://138.201.223.254:8080/yetl1/handle/yetl/4235648
    Collections
    • Journal of Pressure Vessel Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV