dc.description.abstractCold welding defect is the most common defect in electrofusion (EF) joint for connecting polyethylene (PE) pipe. In our previous study [1], the cold welding defect is successfully inspected by an eigenline method based on phased array ultrasonic testing technology. However, limited research has been reported on the acceptance criterion of cold welding defect in EF joint. In this paper, the bonding strength of EF joint is measured using a peeling test. The bonding energy of welding interface is calculated both by phenomenological model and deformation energy analysis method. EF joints with different degrees of cold welding are made and used for peeling tests. The results show that the bonding energy of fused interface rises rapidly after bonding and then goes through a plateau region. The starting point of the plateau region in the bonding energy versus welding time curve is regarded as the minimum required welding time of EF joint. Based on bilinear fitting, the acceptance criterion of cold welding defect is proposed.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleSafety Assessment of Cold Welding Defect in Electro Fusion Joint of Polyethylene Pipe
dc.typeJournal Paper
dc.journal.volume135
dc.journal.issue5
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4024447
dc.journal.fristpage51403
dc.journal.lastpage51403
dc.identifier.eissn1528-8978
dc.treeJournal of Pressure Vessel Technology:;2013:;volume( 135 ):;issue: 005
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record