Show simple item record

dc.contributor.authorJ. Wainstein
dc.contributor.authorJ. Perez Ipiña
dc.date.accessioned2017-05-09T00:54:14Z
dc.date.available2017-05-09T00:54:14Z
dc.date.copyrightFebruary, 2012
dc.date.issued2012
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28556#011403_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/150177
dc.description.abstractCoiled Tubings are thin walled steel tubes of 25–89 mm diameter and thousands meters long, used in the oil industry for production and maintenance services. They suffer plastic deformation during unwinding of the reel, passing through a goosneck arch guide and an injector unit. Strain levels are of 2–3%, making the tubing fail by low cycle fatigue in around 100 wrap–unwrap cycles. As coiled tubing material generally behaves in a ductile manner at surface and down well temperatures, the R curve has to be known to make instability analyses. J-R curves were determined to characterize the fracture toughness of nonused coiled tubing, using nonstandard specimens due to difficulties with their small thickness and diameters. Different crack lengths and crack locations were tested to analyze the 2C0 /W ratio and the influence of the longitudinal weld. The R curves obtained show crack arc length dependence and are influenced by the position of the longitudinal weld.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFracture Toughness of HSLA Coiled Tubing Used in Oil Wells Operations
dc.typeJournal Paper
dc.journal.volume134
dc.journal.issue1
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4004569
dc.journal.fristpage11403
dc.identifier.eissn1528-8978
dc.keywordsTubing
dc.keywordsFracture (Materials)
dc.keywordsFracture toughness AND Thickness
dc.treeJournal of Pressure Vessel Technology:;2012:;volume( 134 ):;issue: 001